Preparation:
Manufacturing Procedure: 1. Heat A up to 40°C under slow mixing to dissolve Dermosoft® 688 Eco. Add A into B under slow mixing 2. Heat separately AB and C up to 75-80°C under slow mixing. 3. Keep B at 75-80°C under slow mixing for 20 minutes to hydrate phospholipids 4. Add C into B under slow mixing. Mix slowly for 5 minutes 5. Increase stirring rate up to maximum level with a rotor stator blender (Silverson) up to 3000 rpm for 3 minutes. 6. Cool down under medium stirring. 7. Add D, E and F below 40°C. 8. Adjust the pH if necessary.Notes:
Formula Specifications: Aspect: Thick, bright, yellow emulsion. Viscosity (RHEO ELV8, Spindle 4, 6 rpm, 3 min): 50 000 - 60 000 mPa.s pH: 5.0 - 5.5 Centrifugation (3000 rpm, 20 min): Stable * = Distributed in France by Lucas Meyer Cosmetics and Unipex Solutions. ** = Non-compliant with Ecocert standards.Disclaimer
While every effort has been made to reproduce these formulations correctly, the Publisher of this website cannot accept any liability for the information presented. All formulations are provided in good faith, but no warranty is given as to accuracy of information or results, or suitability for a particular use, nor is freedom from patent infringement to be inferred. Formulations are offered solely for consideration by the participating manufacturers. Continued use of this web site infers acceptance of this disclaimer.
Latest Issues
SNF, headquartered in Andrézieux, France, is a leading global producer of water-soluble polymers with primary manufacturing sites in France, the USA, and China. Over the last 40 years, SNF has developed expertise in polymer chemistries designed for specialty markets, such as personal care and cosmetics.
SNF’s Personal Care Division offers a...
CITE JAPAN 2025
Pacifico Yokohama
14th - 16th May 2025
NYSCC Suppliers' Day 2025
Javits Center, New York
3rd - 4th June 2025